Construction procedures and specific methods of anti-static table mats

 Anti-static table mats are mainly made of static conductive materials, static dissipative materials and synthetic rubber through a variety of processes. The surface layer is a static dissipative layer about 0.3-0.5 mm thick, and the bottom layer is a conductive layer about 1.5-1.7 mm thick. The table mat has a long-lasting use time, has good anti-acid, anti-alkali, and anti-chemical flux characteristics, and is wear-resistant and easy to clean.


Construction procedures and specific methods

    1. Use cleaning fluid or xylene to clean the waste on the ground (using a cleaning machine)

    2. The thickness of the copper strips used for laying the grounding conductive net is 0.02mm, and the width is 20mm. The number of strips is determined according to the actual width of the ground. ), and at the same time lead one end of the laying copper bar to the outdoor grounding electrode of the earth.

    3. After laying the grounded conductive net, put the anti-static table mats on the ground one by one. If the gap between the table mats is too large, you can cut it straight with a knife to make the gap smaller. Turn the edge of the laid anti-static table mat on the table mat (about 20cm), apply glue (401 glue or double-sided tape) in the middle of the gap, and let it dry for 20-30 minutes. It can be glued immediately), the operation of the bottom surface (black surface) of the anti-static table pad is the same (apply the glue evenly once, and the double-sided tape can be applied to the ground. The bottom surface of the anti-static table pad does not need to be glued with double-sided tape), and then The anti-static table mat is glued to the ground, and then rolled several times with a heavy roller to make the surface of the anti-static table mat neat and straight (if there is a heavy roller, press it by hand or step on it with your foot), and at room temperature It can be used after 48 hours.